Thermal management in grinding of superalloys – A critical review
ABOUT BOOK
Purpose This paper is supposed to provide a critical review of current research progress on thermal management in grinding of superalloys, and future directions and challenges. By understanding the current progress and identifying the developing directions, thermal management can be achieved in the grinding of superalloys to significantly improve the grinding quality and efficiency. Design/methodology/approach The relevant literature is collected from Web of Science, Scopus, CNKI, Google scholar, etc. A total of 185 literature is analyzed, and the findings in the literature are systematically summarized. In this case, the current development and future trends of thermal management in grinding of superalloys can be concluded. Findings The recent developments in grinding superalloys, demands, challenges and solutions are analyzed. The theoretical basis of thermal management in grinding, the grinding heat partition analysis, is also summarized. The novel methods and technologies for thermal management are developed and reviewed, i.e. new grinding technologies and parameter optimization, super abrasive grinding wheel technologies, improved lubrication, highly efficient coolant delivery and enhanced heat transfer by passive thermal devices. Finally, the future trends and challenges are identified. Originality/value Superalloys have excellent physical and mechanical properties, e.g. high thermal stability, and good high-temperature strength. The superalloys have been broadly applied in the aerospace, energy and automobile industries. Grinding is one of the most important precision machining technologies for superalloy parts. Owing to the mechanical and physical properties of superalloys, during grinding processes, forces are large and a massive heat is generated. Consequently, the improvement of grinding quality and efficiency is limited. It is important to conduct thermal management in the grinding of superalloys to decrease grinding forces and heat generation. The grinding heat is also dissipated in time by enhanced heat transfer methods. Therefore, it is necessary and valuable to holistically review the current situation of thermal management in grinding of superalloys and also provide the development trends and challenges.